Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.30 J/cm² @Temperature 23.0 °C |
44.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 9.30 J/cm² | 44.3 ft-lb/in² | ISO 179-1 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 9.30 J/cm² | 44.3 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Charpy Impact Unnotched | 9.30 J/cm² | 44.3 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 9.30 J/cm² | 44.3 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation .. |
|||
Charpy Impact Unnotched | 9.30 J/cm² | 44.3 ft-lb/in² | |
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |