Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.80 J/cm²
41.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1/XCF/20 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Charpy Impact Unnotched 8.80 J/cm²
41.9 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Charpy Impact Unnotched 8.80 J/cm²
41.9 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Charpy Impact Unnotched 8.80 J/cm²
41.9 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics LNP VERTON RX10409D PA 66
LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural.
Charpy Impact Unnotched 8.80 J/cm²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Conditioned, 15% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Charpy Impact Unnotched 8.80 J/cm²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Conditioned, 20% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Charpy Impact Unnotched 8.80 J/cm²
41.9 ft-lb/in²
ISO 179
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Charpy Impact Unnotched 8.80 J/cm²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/2C
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.