Polymer Property : Charpy Impact Unnotched = 33.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 33.0 J/cm²
157 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® II150E BK602 Acetal (POM)
Nucleated High Viscosity Acetal Homopolymer Developed for ExtrusionInformation provided by DuPont Performance Polymers
Charpy Impact Unnotched 33.0 J/cm²
157 ft-lb/in²
50%RH; ISO 179/1eU
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P..