Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.90 J/cm² @Temperature 23.0 °C |
32.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergadur™ PB40 G20 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 6.90 J/cm² | 32.8 ft-lb/in² | Conditioned; ISO 179/1eU |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Charpy Impact Unnotched | 6.90 J/cm² | 32.8 ft-lb/in² | ISO 179 |
BASF Ultramid® C3U BK23079 PA66/6 (Dry) Ultramid C3U BK23079 is an injection molding, general purpose PA66/6, pigmented black grade with improved flame retardance. |