Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® C3U BK23079 PA66/6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® C3U BK23079 PA66/6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultramid C3U BK23079 is an injection molding, general purpose PA66/6, pigmented black grade with improved flame retardance.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Water Absorption 8.5 %
8.5 %
ISO 62
Moisture Absorption at Equilibrium 2.9 %
2.9 %
23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM Data; MD
Mechanical Properties Metric English Comments
Tensile Strength, Yield 84.0 MPa
12200 psi
50mm/min; ISO 527
Elongation at Yield 3.7 %
3.7 %
50mm/min; ISO 527
Tensile Modulus 3.77 GPa
547 ksi
1mm/min; ISO 527
Charpy Impact Unnotched 6.90 J/cm²
32.8 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM Test
Melting Point 243 °C
469 °F
10 K/min
243 °C
469 °F
ASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ISO 75
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Color BK23079
Commercial Status North America and Europe
Impact Modified No
Primary Processing Technique Injection Molding