Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.51 J/cm² | 16.7 ft-lb/in² | EN ISO 179 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |