Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.83 J/cm² @Temperature -30.0 °C |
27.7 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |
|||
Charpy Impact Unnotched | 5.81 J/cm² @Temperature -30.0 °C |
27.7 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Dry) Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp.. |