Mechanical Properties Metric English Comments
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
PolyOne Bergamid™ B700 Mi10 UF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 2002-3 PBT  (Unverified Data**)
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 2401 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 3100-2 PBT, 7.5% Glass Reinforced  (Unverified Data**)
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.7.5% glass-f..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 179/1eU
SYNTHOS Forsan® 846 Acrylonitrile Butadiene Styrene (ABS)
High impact, medium flow, glossy, suitableApplications: General purpose, transport packaging, furniture, leisure time equipmentContainers, suitcases, profiles, ABS sheets, skis, helmets, garden equi..
Charpy Impact Unnotched 19.0 J/cm²
90.4 ft-lb/in²
ISO 179
Styrolution Luran® S 757 G ASA
Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Charpy Impact Unnotched 19.0 J/cm²
90.4 ft-lb/in²
ISO 179
Styrolution Terluran® HH-106 ABS
Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 2002 PBT, Unfilled
Celanex 2002 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002 ia a medium flow material.Information provide..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 2002-2 PBT, Unfilled
Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 2002-3 PBT, Unfilled
Celanex 2002-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-3 is a medium flow material that contains ..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 2401 MT PBT, Medical Technology
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 3100-2 PBT, 7.5% Glass Reinforced
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.Information ..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 3100 7.5% Fiberglass Reinforced Polybutylene Terephthalate
Description: Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Celanex 3109HR is a non-lubricated, 7.5% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties, and processability.7.5% glass filledInform..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Hostaform® S 9362 POM, Impact Modified
Hostaform« acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform« S 9362 provides good impact strength while improving modulus and weld ..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified
Preliminary Data SheetInformation provided by Celanese
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 30.0 °C
90.4 ft-lb/in²

@Temperature 86.0 °F
ISO 179/1eU
Celanese Hostaform® S 9362 XAP2 ™ POM, Impact Modified
Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 2002AP Unreinforced Polybutylene Terephthalate
Description: Celanex 2002AP is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV and heat resistance. Celanex 2002AP is a..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 30.0 °C
90.4 ft-lb/in²

@Temperature 86.0 °F
ISO 179/1eU
Celanese Celanex® 2002UV PBT, Unfilled
Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 2403 MT Unreinforced PBT with Improved Crystallization Speed
Description: Celanex 2403 MT Natural is an unreinforced PBT with improved crystallization speed and faster cycle times that complies with the requirements of the FDA and is listed in the Drug Master..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celcon® M25 POM, Unfilled
Celcon« acetal copolymer grade M25 is a high molecular weight, higher toughness and impact resistance grade primarily used for extrusion and selected injection molding applications.Information prov..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celcon® M25 POM  (Unverified Data**)
Celcon® acetal copolymer grade M25 is a high molecular weight, higher toughness and impact resistance grade primarily used for extrusion and selected injection molding applications.Standard extrude..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Hostaform® S 9362 POM, Impact Modified  (Unverified Data**)
Hostaform® acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform® S 9362 provides good impact strength while improving modulus and weld ..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified  (Unverified Data**)
Preliminary Data SheetImpact modified, improved modulus and weld line, low emissionInformation provided by Celanese
Charpy Impact Unnotched 19.0 J/cm²
90.4 ft-lb/in²
BASF Novolen® 1102 K Polypropylene
Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an..
Charpy Impact Unnotched 19.0 J/cm²
90.4 ft-lb/in²
BASF Novolen® 1104 K Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 19.0 J/cm²
90.4 ft-lb/in²
ISO 179/1eU
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celanex® 2002-2 PBT  (Unverified Data**)
Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a..