Mechanical Properties Metric English Comments
Charpy Impact Unnotched 35.0 J/cm²

@Temperature 23.0 °C
167 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat..
Charpy Impact Unnotched 35.0 J/cm²
167 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions...
Charpy Impact Unnotched 35.0 J/cm²
167 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers with very low ..
Charpy Impact Unnotched 35.0 J/cm²
167 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..
Charpy Impact Unnotched 35.0 J/cm²

@Temperature -30.0 °C
167 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I..
Charpy Impact Unnotched 35.0 J/cm²

@Temperature -40.0 °C
167 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I..
Charpy Impact Unnotched 35.0 J/cm²

@Temperature -30.0 °C
167 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi..