Mechanical Properties Metric English Comments
Charpy Impact Unnotched 34.0 J/cm²

@Temperature -30.0 °C
162 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions ..
Charpy Impact Unnotched 34.0 J/cm²

@Temperature -30.0 °C
162 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..