Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions developed for automotive interior applications. ProcesInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.021 cm/cm
0.021 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.0 MPa
10300 psi
ISO 527-1/-2
Elongation at Break 45 %
45 %
Nominal; ISO 527-1/-2
Elongation at Yield 28 %
28 %
ISO 527-1/-2
Tensile Modulus 2.90 GPa
421 ksi
ISO 527-1/-2
Flexural Modulus 2.80 GPa
406 ksi
ISO 178
Charpy Impact Unnotched 39.0 J/cm²
186 ft-lb/in²
ISO 179/1eU
34.0 J/cm²

@Temperature -30.0 °C
162 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
ISO 75-1/-2
Vicat Softening Point 160 °C
320 °F
50°C/h 50N; ISO 306
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Emissions <2 mg/kg
VDA 275
Part Marking Code >POM<
ISO 11469
Processing Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM
ISO 1043
Special Characteristics Light stabilised or stable to light
U.V. stabilised or stable to weather
Copyright © lookpolymers.com All Rights Reserved