Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -40.0 - -20.0 °C |
>= 143 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 30.0 J/cm² Grade Count:2 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² | >= 143 ft-lb/in² | DIN 53453 |
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature 23.0 °C |
143 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature 23.0 °C |
143 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers, pigmented red, having extremely low VOC emissions, developed for automotive interior applicatio.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LATAN 23 Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 100P BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved ProcessingDelrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100P provides maximum toughness in the product line.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature -30.0 °C |
143 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 300PE NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE NC010 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very .. |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² | 143 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature -30.0 °C |
143 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform N 2640 Z4 UNC Q600 POM Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -40.0 - -20.0 °C |
>= 143 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 30.0 J/cm² Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact Unnotched | 30.0 J/cm² - NB @Temperature -40.0 - -20.0 °C |
143 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 30.0 J/cm² Grade Count:2 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |