Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.39 - 6.50 J/cm² @Temperature -40.0 - 30.0 °C |
6.62 - 30.9 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 3.68 J/cm² Grade Count:66 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Charpy Impact Unnotched | 1.39 J/cm² | 6.61 ft-lb/in² | ISO 179-1 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |