Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 192 J/cm² @Thickness 2.50 mm, Temperature -30.0 °C |
914 ft-lb/in² @Thickness 0.0984 in, Temperature -22.0 °F |
Longitudinal [Cold rolled + Annealed + Pickled, sheet] |
AK Steel 41003 Ferritic Stainless steel AK Steel 41003 is an economical steel that provides excellent weldability, toughness and fabricating characteristics. This alloy is an excellent choice for applications such as tubing and sheet for.. |