Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.81 J/cm²

@Temperature 0.000 °C
8.60 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU 139 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci..