Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Pacific, Europe, South America and North America Features: Balanced Stiffness/ToughnessDuctile Low Temperature Impact Resistance Uses: Automotive BumperAutomotive Exterior PartsAutomotive Exterior TrimProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Melt Flow 13 g/10 min
13 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.0 MPa
1890 psi
ISO 527-2
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527-2
Elongation at Break 52 %
52 %
ISO 527-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 1.30 GPa
189 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.693 J/cm²

@Temperature -30.0 °C
3.30 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
0.798 J/cm²

@Temperature -20.0 °C
3.80 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
1.81 J/cm²

@Temperature 0.000 °C
8.60 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C
120 °F
ISO 75-2/A