Polymer Property : Charpy Impact, Notched = 74.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 15.7 J/cm²

@Temperature -40.0 °C
74.7 ft-lb/in²

@Temperature -40.0 °F
partial break; ISO 179/1eA
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET  (Unverified Data**)
Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size..