Mechanical Properties Metric English Comments
Charpy Impact, Notched 12.2 J/cm²

@Temperature -40.0 °C
58.1 ft-lb/in²

@Temperature -40.0 °F
ISO 179/1eA
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET  (Unverified Data**)
Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon..