Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K-FHG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1/1eA |
Styron Magnumâ„¢ 3525 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3525 is a resin with excellent processing characteristics. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with a stable.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1/1eA |
Styron Magnumâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3325 MT is resin with excellent processing characteristics and a matt surface finish. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent p.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-G6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-HG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-HG6U (Cond.) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-LG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-HG7 (Dry) 35% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TS250F6D Nylon 46-30% Glass Reinforced (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-G6 (Dry) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-HG7 Nylon 66-35% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Conditioned Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.24 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K-FG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnite® TV4 460 KL PBT/PET Blend-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |