Polymer Property : Charpy Impact, Notched = 5.00 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.05 J/cm²

@Temperature 23.0 °C
5.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf..
Charpy Impact, Notched 1.05 J/cm²

@Temperature 23.0 °C
5.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1e
Aardvark Polymers AARTEL® 850IM Rotational Molding Resin
Aartel 850 IM is a moderately toughened impact modified acetal copolymer which exhibits ductility in bending and impact loading. The ductile, rather than brittle, failure mode gives designers more f..
Charpy Impact, Notched 1.05 J/cm²

@Temperature 23.0 °C
5.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced
GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi..
Charpy Impact, Notched 1.05 J/cm²

@Temperature -30.0 °C
5.00 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K224-G4U (Cond.) 23% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.05 J/cm²

@Temperature 23.0 °C
5.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K224-G4U (Cond.) 23% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.05 J/cm²

@Temperature 22.8 °C
5.00 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CNU 015 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin with good stiffness/toughness balance, low odor and emissions, designed for automotive interior applications. Availability: Africa & M..
Charpy Impact, Notched 1.05 J/cm²

@Temperature 22.8 °C
5.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
ExxonMobil PP7033L1 Polypropylene Impact Copolymer
Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like..