Mechanical Properties Metric English Comments
Charpy Impact, Notched 4.90 J/cm²

@Temperature 23.0 °C
23.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin
Dow T710-25 ES Polypropylene Resin DAâ„¢ is a high impact TPO with enhanced flow, scratch and mar, and surface aesthetics for excellent molded-in-color appearance for automotive interior applicat..
Charpy Impact, Notched 4.90 J/cm²

@Temperature -29.0 °C
23.3 ft-lb/in²

@Temperature -20.2 °F
ISO 179
Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin
Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron
Charpy Impact, Notched 4.90 J/cm²

@Temperature 23.0 °C
23.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis Daplen™ EE340AE Polypropylene TPO Compound
Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..