Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.90 J/cm² @Temperature -20.0 °C |
28.1 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 HI/1 PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |