Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.580 J/cm²

@Temperature 23.0 °C
2.76 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A HSK (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.580 J/cm²

@Temperature -30.0 °C
2.76 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® CS 35FL (dry) Nylon 6/66
Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group.