Mechanical Properties Metric English Comments
Charpy Impact, Notched 130 J/cm²

@Temperature 23.0 °C
619 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Arkema Group Rilsan® Clear G170 Polyamide
Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use..
Charpy Impact, Notched 130 J/cm²

@Temperature -30.0 °C
619 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Arkema Group Rilsan® Clear G170 Polyamide
Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use..