Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.320 J/cm² @Temperature 23.0 °C |
1.52 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature 23.0 °C |
1.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 / 1eA |
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature 23.0 °C |
1.52 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A CV300LK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature -30.0 °C |
1.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature 23.0 °C |
1.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Solvay TECHNYL® C 52G1 V20 PA6, DRY Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature -30.0 °C |
1.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Charpy Impact, Notched | 0.320 J/cm² @Temperature -30.0 °C |
1.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3150 MX5 is a high crystallinity and high impact polypropylene (HCPP) copolymer with a Melt Flow index of 15 g/10 min. The material is UV stabilized.Polypropylene PPC 3150 MX5 is .. |