Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.720 J/cm²

@Temperature 23.0 °C
3.43 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® A RV250AF (dry) Nylon 66-25GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..