Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radiflam® A RV250AF (dry) Nylon 66-25GF

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® A RV250AF (dry) Nylon 66-25GF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
Water Absorption 5.6 %
5.6 %
Moisture Absorption at Equilibrium 1.4 %
1.4 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
Elongation at Break 2.5 %
2.5 %
Tensile Modulus 7.90 GPa
1150 ksi
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
0.720 J/cm²

@Temperature 23.0 °C
3.43 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
Vicat Softening Point 240 °C

@Load 5.10 kg
464 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm