Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.370 J/cm² @Temperature 23.0 °C |
1.76 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 610 BT N 32 C PA610 Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 0.370 J/cm² @Temperature -20.0 °C |
1.76 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, C.. |
|||
Charpy Impact, Notched | 0.370 J/cm² @Temperature -30.0 °C |
1.76 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66
(Unverified Data**) Zytel® 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.370 J/cm² @Temperature 23.0 °C |
1.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-3000 B DEL Polypropylene Homopolymer INNOPOL® CS 1-3000 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Charpy Impact, Notched | 0.370 J/cm² @Temperature -30.0 °C |
1.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-GM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.370 J/cm² @Temperature 23.0 °C |
1.76 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Charpy Impact, Notched | 0.370 J/cm² @Temperature -30.0 °C |
1.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Charpy Impact, Notched | 0.370 J/cm² @Temperature -30.0 °C |
1.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |