Plastcom PLASTAMID® 610 BT N 32 C PA610

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer Plastcom spol. s r.o.
Trade Name PLASTAMID®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom PLASTAMID® 610 BT N 32 C PA610.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
STN EN ISO 1183-1
Melt Flow 4.0 g/10 min

@Load 0.325 kg,
Temperature 275 °C
4.0 g/10 min

@Load 0.716 lb,
Temperature 527 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
STN EN ISO 527-2
Elongation at Break 3.5 %
3.5 %
STN EN ISO 527-2
Tensile Modulus 2.60 GPa
377 ksi
STN EN ISO 527-2
Flexural Strength 72.0 MPa
10400 psi
STN EN ISO 178
Flexural Modulus 1.67 GPa
242 ksi
STN EN ISO 178
Charpy Impact Unnotched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
4.50 J/cm²

@Temperature -20.0 °C
21.4 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.360 J/cm²

@Temperature -20.0 °C
1.71 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.370 J/cm²

@Temperature 23.0 °C
1.76 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
STN EN 11357-1
Processing Properties Metric English Comments
Melt Temperature 240 - 260 °C
464 - 500 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.25 %
0.25 %
STN EN ISO 3344
Descriptive Properties Value Comments
Color Natural