Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.13 J/cm | 9.60 ft-lb/in | ASTM D256 |
Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant HCR-125 is a corrosion resistant vinyl ester sheet created by impregnating fiber glass mat, synthetic surface veil, and inert additives with Derkane 470 resin and catalyst. A compression molded pro.. |