Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.13 J/cm | 9.60 ft-lb/in | ASTM D256 |
Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant HCR-125 is a corrosion resistant vinyl ester sheet created by impregnating fiber glass mat, synthetic surface veil, and inert additives with Derkane 470 resin and catalyst. A compression molded pro.. |
|||
Izod Impact, Notched | 5.13 J/cm @Temperature -30.0 °C |
9.61 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |