Polymer Property : Izod Impact, Notched = 9.14 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.88 J/cm
9.14 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP 2FL24 ETFE
LNP* THERMOCOMP* 2FL24 is a compound based on ETFE resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is Wear Resistant.
Izod Impact, Notched 4.88 J/cm

@Temperature 23.0 °C
9.14 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE)
LNP* 2FL24 is a Fluoropolymer, ETFE grade containing Glass Fibers and PTFE.This data was supplied by SABIC-IP for the Americas region.