Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.694 - 4.70 J/cm | 1.30 - 8.81 ft-lb/in | Average value: 1.78 J/cm Grade Count:49 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |