Polymer Property : Izod Impact, Notched = 8.43 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.43 J/cm

@Temperature 23.0 °C
15.8 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX GTX6010 PPE+PA6 (Asia Pacific)
PA6 based unfilled GTX. High impact.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 8.43 J/cm
15.8 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific)
PA6 based unfilled GTX. High impact.