SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA6 based unfilled GTX. High impact.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Thickness 3.20 mm
0.011 - 0.013 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
SABIC - Japan Method
Elongation at Break 150 %
150 %
SABIC - Japan Method
Flexural Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 8.43 J/cm
15.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 80.0 - 100 µm/m-°C

@Temperature -30.0 - 30.0 °C
44.4 - 55.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 180 °C

@Thickness 3.20 mm
356 °F

@Thickness 0.126 in
unannealed; ASTM D648