Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 7.28 J/cm | 13.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |