Mechanical Properties Metric English Comments
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Izod Impact, Notched 6.99 J/cm
13.1 ft-lb/in
Reliance Industries PBT - 35% Glass filled
Information provided by Reliance Industries
Izod Impact, Notched 6.99 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRILOY D20009 PC
LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Flame Retardant, Wear Resistant.
Izod Impact, Notched 6.99 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific)
LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer