Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.73 J/cm @Thickness 6.35 mm |
6.98 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.73 J/cm @Thickness 6.35 mm |
6.98 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |