Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.04 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
5.69 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical |