Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.55 J/cm | 10.4 ft-lb/in | CW; ASTM D257 |
Haysite H1000 Polyester Laminate Haysite Grade 1000 laminate sheet is an outstanding material that is used in applications requiring exceptional weather and corrosion resistance. Grade H1000's unique polyester resin system provide.. |
|||
Izod Impact, Notched | 5.55 J/cm @Thickness 3.20 mm |
10.4 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5301 PEI 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 5.55 J/cm @Thickness 3.20 mm |
10.4 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5301 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 5.55 - 6.62 J/cm | 10.4 - 12.4 ft-lb/in | |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |