Polymer Property : Izod Impact, Notched = 5.14 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.75 J/cm
5.14 ft-lb/in
ASTM D256 A
GRECO ISOPAK 547 ABS Resin
High Impact GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Izod Impact, Notched 2.75 J/cm

@Thickness 3.17 mm
5.14 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact
High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.75 J/cm

@Thickness 3.17 mm
5.14 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact
High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.75 J/cm

@Thickness 3.17 mm
5.14 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Tramid® 215 Polyamide, High Impact
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.215 is a high impact grade.Applications:Automotive knob types, door handles and m..