Material Notes:
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.215 is a high impact grade.Applications:Automotive knob types, door handles and mirror housingsConnectorsCable tiesHarness clipsTubesFastenersCastor wheelsHose clipsVacuum hoseHood stayInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 1.4 %
1.4 %
ASTM D570
Linear Mold Shrinkage 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 53.9 MPa
7820 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 6.47 GPa
939 ksi
ASTM D790
Izod Impact, Notched 2.75 J/cm

@Thickness 3.17 mm
5.14 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 214 °C
417 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648