Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.34 J/cm | 4.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD000P PC LNP* STAT-KON* DD000P is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
Izod Impact, Notched | 2.34 J/cm | 4.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific) LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
Izod Impact, Notched | 2.34 J/cm | 4.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX0844 PPE+PS PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability. |
|||
Izod Impact, Notched | 2.34 J/cm | 4.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX0844 PPE+PS (Asia Pacific) Automotive interiors. High heat/moisture resistant. consistant processability. |
|||
Izod Impact, Notched | 2.34 J/cm | 4.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON PX91060 PA 6 LNP* VERTON* PX91060 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added feature of this grade is: Structural. |
|||
Izod Impact, Notched | 2.34 J/cm | 4.38 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON PX91060 PA 6 (Asia Pacific) LNP* Verton* PX91060 is a compound based on Nylon 6 resin containing Long Glass Fiber. |