Mechanical Properties Metric English Comments
Izod Impact, Notched 4.21 J/cm
7.89 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® EX75 ABS
Multi-purpose, extrusion ABS providing a favorable balance of engineering properties.
Izod Impact, Notched 4.21 J/cm
7.89 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopoly (Asia Pacific)
LNP* Thermocomp* KF004AL is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Izod Impact, Notched 4.21 J/cm
7.89 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopolymer
LNP* THERMOCOMP* KF004AL is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. Added features of this material include: Low Extractible.