SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopoly (Asia Pacific)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Glass Fiber Reinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopoly (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* KF004AL is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 3.7 %
3.7 %
ASTM D638
Tensile Modulus 8.61 GPa
1250 ksi
50 mm/min; ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 4.21 J/cm
7.89 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 149 °C

@Thickness 3.20 mm
300 °F

@Thickness 0.126 in
unannealed; ASTM D648