Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.85 J/cm @Temperature -30.0 °C |
7.21 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press. |
|||
Izod Impact, Notched | 3.85 J/cm | 7.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material. |
|||
Izod Impact, Notched | 3.85 J/cm | 7.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Izod Impact, Notched | 3.85 J/cm | 7.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Izod Impact, Notched | 3.85 J/cm | 7.21 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |