Mechanical Properties Metric English Comments
Izod Impact, Notched 2.78 - 3.84 J/cm
5.20 - 7.20 ft-lb/in
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound
BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr..