Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intricate parts. Typical applications are circuit breakers, insulators, bobbins and electrical connectors.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.87 - 2.07 g/cc
0.0676 - 0.0748 lb/in³
Molded
Linear Mold Shrinkage 0.0017 - 0.0022 cm/cm
0.0017 - 0.0022 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength 57.2 - 71.0 MPa
8300 - 10300 psi
Flexural Strength 116 - 143 MPa
16800 - 20800 psi
Flexural Modulus 8.96 - 10.3 GPa
1300 - 1500 ksi
Compressive Strength 162 - 190 MPa
23500 - 27500 psi
Izod Impact, Notched 2.78 - 3.84 J/cm
5.20 - 7.20 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 13.8 - 15.8 kV/mm
351 - 401 kV/in
short time
Arc Resistance >= 181 sec
>= 181 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F