Mechanical Properties Metric English Comments
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D-256
PlastiComp Velocity® LCF50-PA66 High Flow Nylon 66, 50% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.20 mm
3.41 ft-lb/in

@Thickness 0.126 in
ASTM D256
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.20 mm
3.41 ft-lb/in

@Thickness 0.126 in
ASTM D256
NOVA Chemicals Novapol® TR-0338-U MDPE Rotational Molding Resin  (discontinued **)
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66
LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare.
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM Data
Dow C702-20 Polypropylene Impact Copolymer
Dow Polypropylene Impact Copolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resis..
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 261WO PPO
A general purpose V-0 rated resin with good impact strength.Data provided by the manufacturer
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 527LD-33G Nylon 66, High Impact, 33% Glass Reinforced
A high impact reinforced Nylon 66 with good low temperature properties.Data provided by the manufacturer
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 559LD-33G Nylon 66, 33% Glass Reinforced
A high impact reinforced nylon copolymer with good low temperature properties.Data provided by the manufacturer
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 727 Nylon 6
A modified nylon for applications requiring flexibility.Data provided by the manufacturer
Izod Impact, Notched 1.82 J/cm

@Thickness 3.20 mm
3.41 ft-lb/in

@Thickness 0.126 in
ASTM D256
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin  (discontinued **)