Mechanical Properties Metric English Comments
Izod Impact, Notched 1.73 J/cm
3.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Izod Impact, Notched 1.73 J/cm
3.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific)
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.